Tue Oct 30 18:35:51 2012, Christian Irmler, MicronOrigami_gross, run, run040, 100k, 30.10.2012 18:23:21, 30.10.2012 21:55:53 , Unknown
|
Cooling for 2DSSD established after some struggle.
2DSSD fully read out with cooling
HV= +40 V -40 V I = 2.1 uA
Beam position:
Origami -z
p-side: APV #5
n-side: APV #13 (= pos.1 of -z)
Positions of thermal sensors:
11 Kapillare Anfang
12 Kapillare Ende
13 ---
14 unmittelbar nach Kapillare
15 Origami in
16 Origami out
17 Origami -z
18 Origami CE
Strip order:
n-Seite: rechts (Salev) nach links (Jura)
p-Seite: oben nach unten
APV chips with lower noise:
-z ce
p-side #5 #10 (= pos 4)
n-side #13 (= pos1) #19 (= pos 3) |
Tue Oct 30 17:24:01 2012, Markus Friedl, MicronOrigami_gross, cal, cal040, 83800, 30.10.2012 17:20:28 , 30.10.2012 17:54:09, Unknown
|
Cooling for 2DSSD established after some struggle.
2DSSD fully read out with cooling
HV= +40 V -40 V I = 2 uA
Beam position: none
Positions of thermal sensors:
11 Kapillare Anfang
12 Kapillare Ende
13 ---
14 unmittelbar nach Kapillare
15 Origami in
16 Origami out
17 Origami -z
18 Origami CE
Strip order:
n-Seite: rechts (Salev) nach links (Jura)
p-Seite: oben nach unten
APV chips with lower noise:
-z ce
p-side #5 #10 (= pos 4)
n-side #13 (= pos1) #19 (= pos 3)
|
Tue Oct 30 11:05:32 2012, Markus Friedl, HPK_baby, run, run039, 150k, 30.10.2012 11:03:19, 30.10.2012 14:57:57, Unknown
|
HPK baby stack after irradiation - no cooling
I = 420A and growing (warming up)
positioned centered on p and n
|
Tue Oct 30 10:37:19 2012, Markus Friedl, HPK_baby, cal, cal039, 83800, 30.10.2012 10:35:35 , 30.10.2012 11:02:06 , Good
|
Turned off cooling, now taking warm data
HPK baby stack after irradiation - no cooling
I = 200A and growing (warming up)
positioned centered on p and n
|
Mon Oct 29 23:13:52 2012, Markus Friedl, HPK_baby, run, run038, 476500, 29.10.2012 23:13:05, 30.10.2012 10:22:54, Unknown
|
HPK baby stack after irradiation with partial cooling (HPK neutron & HPK neutron/gamma)
HV = +75 V -75V
I = 176A
positioned centered on p and n
Temp sensors configuration:
11 HPK Neutron n in
12 HPK Neutron n -> p
13 ----
14 HPK Neutron p -> Gamma p
15 Gamma p -> n
16 Neutron Gamma n out
Perfect cooling curve :-)
|
Mon Oct 29 22:36:52 2012, Markus Friedl, HPK_baby, cal, cal038, 83800, 29.10.2012 22:17:34, 29.10.2012 22:47:47, Good
|
HPK baby stack after irradiation with partial cooling (HPK neutron & HPK neutron/gamma)
HV = +75 Vm -75V
I = 226A
Temp sensors configuration:
11 HPK Neutron n in
12 HPK Neutron n -> p
13 ----
14 HPK Neutron p -> Gamma p
15 Gamma p -> n
16 Neutron Gamma n out |
Mon Oct 29 12:24:41 2012, Markus Friedl, Infineon, run, run037, 301382, 29.10.2012 12:22:22, 29.10.2012 21:05:57, Good
|
Infineon stack Version 2 after irradiation
HV = +300 V
I = 162 A
hitting upper part of strixels and baby, vertically ~centered |
Mon Oct 29 11:36:40 2012, Markus Friedl, Infineon, cal, cal037, 83800, 29.10.2012 11:35:12, 29.10.2012 11:58:02 , Good
|
Infineon stack Version 2 after irradiation
HV = +300 V
I = 137 A
|
Mon Oct 29 04:02:16 2012, Manfred Valentan, MicronBaby, run, run036, 296294, 29.10.2012 03:53:33, 29.10.2012 11:05:35, Unknown
|
Micron Baby stack 2 after irradiation (intermediate strips)
HV = -100 V
I = 36 uA
DESY table shifted by 2.5mm (beam down) after beam profile was changed (to get higher intensity)
beam hitting higher APVs
Stopped when long beam off period was announced |
Sun Oct 28 20:07:28 2012, Markus Friedl, MicronBaby, run, run035, 304110, 28.10.2012 20:01:48, 29.10.2012 03:50:44, Good
|
Micron Baby stack 2 after irradiation (intermediate strips)
HV = -100 V
I = 39 uA
DESY table shifted by 2.5mm (beam down) after beam profile was changed (to get higher intensity)
beam hitting lower APVs |
Sun Oct 28 16:22:35 2012, Christian Irmler, MicronBaby, run, run034, 101864, 28.10.2012 16:12:24 , 28.10.2012 18:34:24, Good
|
Micron Baby stack 2 after irradiation (intermediate strips)
HV = -100 V
I = 36.3 uA
Position APV0 of all sensors
X-Y Table coordinates:
X=0 / Y=-1 (afterwards: nulled)
PC power cut after ~100k events |
Sun Oct 28 15:46:07 2012, Markus Friedl, MicronBaby, cal, cal034, 83800, 28.10.2012 15:19:10, 28.10.2012 15:40:47, Good
|
Micron Baby stack 2 after irradiation (intermediate strips)
HV = -100 V
I = 33 uA |
Sun Oct 28 08:37:53 2012, Christian Irmler, MicronOrigami_gross, run, run033, 66937, 28.10.2012 08:33:42, 28.10.2012 14:10:43 , Unknown
|
Belle stack 2 after gamma irradiation
HV = +50V -50V
I = 101 uA
CO2 cooling
hitting APV2 (n side) = center of wedge sensor
Temperatur sensors:
- T11: Origami #4 in
- T12: Origami #4 out
- T13: Origami #3 in (still wrong values!)
- T14: Origami #3 out
- T15: Wedge new 1 out
- T16: Wedge old out
- T17: Wedge new 1 cooling block
- T18: Wedge old cooling block
|
Sun Oct 28 02:51:49 2012, Markus Friedl, MicronOrigami_gross, run, run032, 150k, 28.10.2012 02:47:24, 28.10.2012 08:31:19 , Good
|
Belle stack 2 after gamma irradiation
HV = +50V -50V
I = 101 uA
Bias currents absolutely stable during the whole run.
CO2 cooling
hitting APV3 (n side) = wide side of wedge sensor |
Sat Oct 27 21:49:08 2012, Markus Friedl, MicronOrigami_gross, run, run031, 150k, 27.10.2012 21:42:46, 28.10.2012 02:35:55 (+1h due to winter time), Good
|
Belle stack 2 after gamma irrdiation
HV = +50V -50 V
I = 102 uA
CO2 cooling
|
Sat Oct 27 19:36:24 2012, Markus Friedl, MicronOrigami_gross, cal, cal031, 83800, 27.10.2012 19:59:50, 27.10.2012 20:44:38, Good
|
Belle stack 2 after irradiation
HV = +50V -50V
I = 112 µA
CO2 cooling |
Sat Oct 27 07:51:49 2012, Manfred Valentan, MicronBaby, run, run030, 376678, 27.10.2012 07:49:09, 27.10.2012 17:32:07, Good
|
After irradiation
xy-table: x=319.4, y=87.6
beam hits APV1
Micron baby stack after gamma irrdiation
HV = -100 V
I = -58 uA |
Sat Oct 27 01:13:47 2012, Christian Irmler, MicronBaby, run, run029, 307k, 27.10.2012 01:02:49, 27.10.2012 07:36:34, Good
|
After irradiation
xy-table: x=319.4, y=74.6
beam hits APV0
Micron baby stack after gamma irrdiation
HV = -100 V
I = -58 uA |
Sat Oct 27 00:43:55 2012, Christian Irmler, MicronBaby, cal, cal029, 83800, 27.10.2012 00:10:15, 27.10.2012 00:36:55, Good
|
After irradiation
Micron baby stack after gamma irrdiation
HV = -100 V
I = -58 uA |
Wed Oct 24 09:51:41 2012, Thomas Bergauer, MicronOrigami_gross, cal, cal028, 83800, 24.10.2012 09:50:53, 24.10.2012 10:39:43, Unknown
|
Belle Stack 4: 2 DSSD -z, Origami #3, #1, wedge new #2
HV = +-2.5V, Ibias=14.5uA
Position: APVs #2, 7, 11, 15 | # 17/18, 21, 25, 29