| ID  | Date | Author | Project | Measurement Type | Object ID | Subject | 
| 26 | Thu May  8 16:51:03 2014 | Benedikt Würkner | Belle II | source | L3 module | No 1 of 6 room temperature measurements using Sr90 Source (single) | 
| Sr90 Radioactive SourceNo cooling
 Module position: 0:0(top left)
 HV Turned to +40,-40V with currents. +1.0 and -1.0 µA
 
 N+1.25V current: 0.22A
 N+2.50V current: 0.57A
 P+1.25V current: 0.26A
 P+2.50V current: 0.72A
 
 Events: 200000
 | 
| Attachment 1: run07_all_hits_apv0.png | 
|  | 
| Attachment 2: run07_all_hits_apv1.png | 
|  | 
| Attachment 3: run07_all_hits_apv2.png | 
|  | 
| Attachment 4: run07_all_hits_apv3.png | 
|  | 
| Attachment 5: run07_all_hits_apv4.png | 
|  | 
| Attachment 6: run07_all_hits_apv5.png | 
|  | 
| Attachment 7: run07_all_hits_apv6.png | 
|  | 
| Attachment 8: run07_all_hits_apv7.png | 
|  | 
| Attachment 9: run07_all_hits_apv8.png | 
|  | 
| Attachment 10: run07_all_hits_apv9.png | 
|  | 
| 23 | Wed May  7 18:20:36 2014 | Benedikt Würkner | Belle II | source | L3 module | No 6 of 6 room temperature measurements using Sr90 Source (multi6) | 
| Sr90 Radioactive SourceNo cooling
 Module position: -57:-30(bottom right)
 HV Turned to +40,-40V with currents. +1.2 and -1.22 µA
 
 N+1.25V current: 0.22A
 N+2.50V current: 0.56A
 P+1.25V current: 0.26A
 P+2.50V current: 0.70A
 
 Events: 200000
 | 
| Attachment 1: run06_all_hits_apv0.png | 
|  | 
| Attachment 2: run06_all_hits_apv1.png | 
|  | 
| Attachment 3: run06_all_hits_apv2.png | 
|  | 
| Attachment 4: run06_all_hits_apv3.png | 
|  | 
| Attachment 5: run06_all_hits_apv4.png | 
|  | 
| Attachment 6: run06_all_hits_apv5.png | 
|  | 
| Attachment 7: run06_all_hits_apv6.png | 
|  | 
| Attachment 8: run06_all_hits_apv7.png | 
|  | 
| Attachment 9: run06_all_hits_apv8.png | 
|  | 
| Attachment 10: run06_all_hits_apv9.png | 
|  | 
| 22 | Wed May  7 17:33:21 2014 | Benedikt Würkner | Belle II | source | L3 module | No 5 of 6 room temperature measurements using Sr90 Source (multi6) | 
| Sr90 Radioactive SourceNo cooling
 Module position: -32:-30(bottom center)
 HV Turned to +40,-40V with currents. +1.22 and -1.24 µA
 
 N+1.25V current: 0.22A
 N+2.50V current: 0.56A
 P+1.25V current: 0.26A
 P+2.50V current: 0.70A
 
 Events: 200000
 | 
| Attachment 1: run05_all_hits_apv0.png | 
|  | 
| Attachment 2: run05_all_hits_apv1.png | 
|  | 
| Attachment 3: run05_all_hits_apv2.png | 
|  | 
| Attachment 4: run05_all_hits_apv3.png | 
|  | 
| Attachment 5: run05_all_hits_apv4.png | 
|  | 
| Attachment 6: run05_all_hits_apv5.png | 
|  | 
| Attachment 7: run05_all_hits_apv6.png | 
|  | 
| Attachment 8: run05_all_hits_apv7.png | 
|  | 
| Attachment 9: run05_all_hits_apv8.png | 
|  | 
| Attachment 10: run05_all_hits_apv9.png | 
|  | 
| 21 | Wed May  7 16:43:37 2014 | Benedikt Würkner | Belle II | source | L3 module | No 4 of 6 room temperature measurements using Sr90 Source (multi6) | 
| Sr90 Radioactive SourceNo cooling
 Module position: -5:-30(bottom left)
 HV Turned to +40,-40V with currents. +1.25 and -1.26 µA
 
 N+1.25V current: 0.22A
 N+2.50V current: 0.57A
 P+1.25V current: 0.26A
 P+2.50V current: 0.72A
 
 Events: 200000
 | 
| Attachment 1: run04_all_hits_apv0.png | 
|  | 
| Attachment 2: run04_all_hits_apv1.png | 
|  | 
| Attachment 3: run04_all_hits_apv2.png | 
|  | 
| Attachment 4: run04_all_hits_apv3.png | 
|  | 
| Attachment 5: run04_all_hits_apv4.png | 
|  | 
| Attachment 6: run04_all_hits_apv5.png | 
|  | 
| Attachment 7: run04_all_hits_apv6.png | 
|  | 
| Attachment 8: run04_all_hits_apv7.png | 
|  | 
| Attachment 9: run04_all_hits_apv8.png | 
|  | 
| Attachment 10: run04_all_hits_apv9.png | 
|  | 
| 20 | Wed May  7 15:53:38 2014 | Benedikt Würkner | Belle II | source | L3 module | No 3 of 6 room temperature measurements using Sr90 Source (multi6) | 
| Sr90 Radioactive SourceNo cooling
 Module position: -59:-20(top right)
 HV Turned to +40,-40V with currents. +1.25 and -1.26 µA
 
 N+1.25V current: 0.22A
 N+2.50V current: 0.56A
 P+1.25V current: 0.26A
 P+2.50V current: 0.71A
 
 Events: 200000
 | 
| Attachment 1: run03_all_hits_apv0.png | 
|  | 
| Attachment 2: run03_all_hits_apv1.png | 
|  | 
| Attachment 3: run03_all_hits_apv2.png | 
|  | 
| Attachment 4: run03_all_hits_apv3.png | 
|  | 
| Attachment 5: run03_all_hits_apv4.png | 
|  | 
| Attachment 6: run03_all_hits_apv5.png | 
|  | 
| Attachment 7: run03_all_hits_apv6.png | 
|  | 
| Attachment 8: run03_all_hits_apv7.png | 
|  | 
| Attachment 9: run03_all_hits_apv8.png | 
|  | 
| Attachment 10: run03_all_hits_apv9.png | 
|  | 
| 19 | Wed May  7 15:04:32 2014 | Benedikt Würkner | Belle II | source | L3 module | No 2 of 6 room temperature measurements using Sr90 Source (multi6) | 
| Sr90 Radioactive SourceNo cooling
 Module position: -32:-20(top center)
 HV Turned to +40,-40V with currents. +1.23 and -1.25 µA
 
 N+1.25V current: 0.22A
 N+2.50V current: 0.56A
 P+1.25V current: 0.26A
 P+2.50V current: 0.71A
 
 Events: 200000
 | 
| Attachment 1: run02_all_hits_apv0.png | 
|  | 
| Attachment 2: run02_all_hits_apv1.png | 
|  | 
| Attachment 3: run02_all_hits_apv2.png | 
|  | 
| Attachment 4: run02_all_hits_apv3.png | 
|  | 
| Attachment 5: run02_all_hits_apv4.png | 
|  | 
| Attachment 6: run02_all_hits_apv5.png | 
|  | 
| Attachment 7: run02_all_hits_apv6.png | 
|  | 
| Attachment 8: run02_all_hits_apv7.png | 
|  | 
| Attachment 9: run02_all_hits_apv8.png | 
|  | 
| Attachment 10: run02_all_hits_apv9.png | 
|  | 
| 18 | Wed May  7 14:36:29 2014 | Benedikt Würkner | Belle II | source | L3 module | No 1 of 6 room temperature measurements using Sr90 Source (multi6) | 
| Sr90 Radioactive SourceNo cooling
 Module position: -5:-20(top left)
 HV Turned to +40,-40V with currents. +1.2 and -1.2 µA
 
 N+1.25V current: 0.22A
 N+2.5 V current: 0.56A
 P+1.25V current: 0.26A
 P+2.50V current: 0.70A
 
 Events: 200000
 | 
| Attachment 1: run01_all_hits_apv0.png | 
|  | 
| Attachment 2: run01_all_hits_apv1.png | 
|  | 
| Attachment 3: run01_all_hits_apv2.png | 
|  | 
| Attachment 4: run01_all_hits_apv3.png | 
|  | 
| Attachment 5: run01_all_hits_apv4.png | 
|  | 
| Attachment 6: run01_all_hits_apv5.png | 
|  | 
| Attachment 7: run01_all_hits_apv6.png | 
|  | 
| Attachment 8: run01_all_hits_apv7.png | 
|  | 
| Attachment 9: run01_all_hits_apv8.png | 
|  | 
| Attachment 10: run01_all_hits_apv9.png | 
|  | 
| 17 | Sun Jul  4 05:48:36 2010 | Christian Irmler | BELLE Upgrade | source | Origami 6 - module 1 | run002: first analysis results | 
| Run name: run002
 Run type: 0 (Hardware (Normal Run))
 Comments:
 After ~40min warmup
 HV=80
 90Sr 1mCi source - moved compared to run001
 multi6
 
 Max. Events=100000      Trg delay=25
 Origami 6 module #1w/o cooling
 sensor: B2HPK_10938-9239_8
 n-side: all 4 APVs read outp-side: APV #0 to #3  read out, analog output of #4 and #5 were not connected to FADC board
     | 
| Attachment 1: run002_cluster_sum.txt | 
| Analysis of run002
Peak Mode, 3 x 200 initevents (first 10 skipped) + 99400 events
Number hybrids:  2	number zones:  2	 number sensors:  1
Using calibration file intcal001
No pedestal correction file
Seed/Neighbor/Cluster/Noisy Strips Cuts [RMS noise]: 5.0/3.0/5.0
Min. hitlength:   3
Comments:
After ~40min warmup
HV=80
90Sr 1mCi source - moved compared to run001
multi6
Analysis date: 04.07.2010 05:40:47
Analysis settings:
 runname: run002_cluster
 clock: 40.00 MHz
 datafilepath: ./
 outputpath: ./
 subevents:  6
 fitmode: 2 (cal. fit)
 options: hr
Results:
ModuleName           ZoneType    Ch    OKCh     OK%   Entries    MClW    MPSignal   Noise   MPSNR   HpSE  Occup SigSlop SigInt SigRes PtiSlop PtiInt  PtiRes ClwSlop ClwInt  ClwRes
Origami6_mod1_p   Orgami 6"    512    512   100.0     34659    1.87    24436.5   3330.4    6.74   0.25   0.80   0.95   0.00  6651.0   1.00   -17.63   7.47    1.00    0.21   0.86
Origami6_mod1_n   Orgami 6"    512    508    99.2     95601    1.93    23801.7    962.7   17.08   1.02   0.79   0.95   0.00  6651.0   1.00   -17.63   7.47    1.00    0.21   0.86
 | 
| Attachment 2: run002_cluster_noi_0.ps | 
| Attachment 3: run002_cluster_sig_0.ps | 
| Attachment 4: run002_cluster_hit_0.ps | 
| Attachment 5: run002_cluster_hpt_0.ps | 
| Attachment 6: run002_cluster_clw_0.ps | 
| Attachment 7: run002_cluster_cor_0.ps | 
| 16 | Wed Oct  7 14:24:06 2009 | Dieter Uhl | BELLE Upgrade | hybrid | #5 | hybrid-pitchadapter | 
| shorts at upper coat 
   opens at upper coat 
   shorts at lower coat 
   opens at lower coat 
 | 
| 15 | Wed Oct  7 14:23:35 2009 | Dieter Uhl | BELLE Upgrade | hybrid | #4 | hybrid-pitchadapter | 
| opens at upper coat 
   shorts at upper coat 
   opens at lower coat 
   shorts at lower coat 
 | 
| 14 | Tue May 20 14:27:50 2008 | Markus Friedl | BELLE Upgrade | source | micron | analysis results of source test | 
| 
*** NOTE: AFTER THIS MEASUREMENT WE REALIZED THAT BIASING WAS NOT DONE PROPERLY
          HENCE THE RESULTS BELOW ARE NOT RELIABLE 
          (in fact it is surprising that they are not worse) ***
Please find the results of the lab source test on the new Micron module here.
It is read out with 3 + 3 APV chips on either side.
Results table of the source measurement:
                      p-side     n-side
 Cluster signal [e]    18361      19434
 Strip noise [e]        1142       1193
 Avg cluster width      1.91       1.30
 Single strip SNR       16.1       16.3
 Cluster SNR            11.6       14.3
 Strip pitch [um]       50.0      153.5     
Apparently, the double metal capacitance is not so bad as expected, even though the Micron sensor does not use
the hourglass crossing scheme. Presumably the dielectric between metal 1 and 2 is rather thick (several um).
Strip noise is roughly the same on both p and n side, so the difference in Cluster SNR (*) only stems from the
unequal cluster width (which is a result of the different pitches).
Peak time precision vs SNR (last plot below) is worse compared to the values obtained with various HPK sensors
in the November 2007 beam test at KEK. However, this is a comparison of source and beam and thus might not be
significant. Let's see what we will get in the SPS beam test next week.
(*) Cluster SNR := sum(signal) / (strip_noise * sqrt(cluster_width) ) | 
| Attachment 1: vie_micron_run002_signal.gif | 
|  | 
| Attachment 2: vie_micron_run002_noise.gif | 
|  | 
| Attachment 3: vie_micron_run002_hit.gif | 
|  | 
| Attachment 4: vie_micron_run002_clw.gif | 
|  | 
| Attachment 5: vie_micron_p_run002_tres.gif | 
|  | 
| Attachment 6: vie_micron_n_run002_tres.gif | 
|  | 
| Attachment 7: vie_micron_p_run002_ressnr.gif | 
|  | 
| Attachment 8: vie_micron_n_run002_ressnr.gif | 
|  | 
| Attachment 9: trms_vs_snr_micron_src.gif | 
|  | 
| 13 | Fri May  9 10:04:26 2008 | Christian Irmler | SPS Testbeam June08 | module | module 05/05 | properties (noise, intcal), APVs bonded to the sensor | 
| Module tested with 1 and 2 rows bonded to the sensor, respectively. 
HV = 100 V
Ibias (100 V) = 18.0 nA
Ibias (200 V) = 23.6 nA | 
| Attachment 1: modul0505_1row_cal_apv0.png | 
|  | 
| Attachment 2: modul0505_1row_cal_apv1.png | 
|  | 
| Attachment 3: modul0505_1row_cmnoise_apv0.png | 
|  | 
| Attachment 4: modul0505_1row_cmnoise_apv1.png | 
|  | 
| Attachment 5: modul0505_1row_pednoise_apv0.png | 
|  | 
| Attachment 6: modul0505_1row_pednoise_apv1.png | 
|  | 
| Attachment 7: modul0505_final_cal_apv0.png | 
|  | 
| Attachment 8: modul0505_final_cal_apv1.png | 
|  | 
| Attachment 9: modul0505_final_cmnoise_apv0.png | 
|  | 
| Attachment 10: modul0505_final_cmnoise_apv1.png | 
|  | 
| Attachment 11: modul0505_final_pednoise_apv0.png | 
|  | 
| Attachment 12: modul0505_final_pednoise_apv1.png | 
|  | 
| 12 | Fri May  9 10:00:34 2008 | Christian Irmler | SPS Testbeam June08 | module | module 03/10 | properties (noise, intcal), APVs bonded to the sensor | 
| Module tested with 1 and 2 rows bonded to the sensor, respectively. 
HV = 100 V
Ibias (100 V) = 18.9 nA
Ibias (200 V) = 25.5 nA | 
| Attachment 1: modul0310_1row_cal_apv0.png | 
|  | 
| Attachment 2: modul0310_1row_cal_apv1.png | 
|  | 
| Attachment 3: modul0310_1row_cmnoise_apv0.png | 
|  | 
| Attachment 4: modul0310_1row_cmnoise_apv1.png | 
|  | 
| Attachment 5: modul0310_1row_pednoise_apv0.png | 
|  | 
| Attachment 6: modul0310_1row_pednoise_apv1.png | 
|  | 
| Attachment 7: modul0310_final_cal_apv0.png | 
|  | 
| Attachment 8: modul0310_final_cal_apv1.png | 
|  | 
| Attachment 9: modul0310_final_cmnoise_apv0.png | 
|  | 
| Attachment 10: modul0310_final_cmnoise_apv1.png | 
|  | 
| Attachment 11: modul0310_final_pednoise_apv0.png | 
|  | 
| Attachment 12: modul0310_final_pednoise_apv1.png | 
|  | 
| 11 | Fri May  9 09:56:15 2008 | Christian Irmler | SPS Testbeam June08 | module | module 06/03 | properties (noise, intcal), APVs bonded to the sensor | 
| Module tested with 1 and 2 rows bonded to the sensor, respectively. 
HV = 100 V
Ibias (100 V) = 26.5 nA
Ibias (200 V) = 37.8 nA | 
| Attachment 1: modul0603_1row_cal_apv0.png | 
|  | 
| Attachment 2: modul0603_1row_cal_apv1.png | 
|  | 
| Attachment 3: modul0603_1row_cmnoise_apv0.png | 
|  | 
| Attachment 4: modul0603_1row_cmnoise_apv1.png | 
|  | 
| Attachment 5: modul0603_1row_pednoise_apv0.png | 
|  | 
| Attachment 6: modul0603_1row_pednoise_apv1.png | 
|  | 
| Attachment 7: modul0603_final_cal_apv0.png | 
|  | 
| Attachment 8: modul0603_final_cal_apv1.png | 
|  | 
| Attachment 9: modul0603_final_cmnoise_apv0.png | 
|  | 
| Attachment 10: modul0603_final_cmnoise_apv1.png | 
|  | 
| Attachment 11: modul0603_final_pednoise_apv0.png | 
|  | 
| Attachment 12: modul0603_final_pednoise_apv1.png | 
|  | 
| 10 | Wed May  7 19:05:08 2008 | Christian Irmler | SPS Testbeam June08 | module | module 04/04 | properties (noise, intcal), APVs bonded to the sensor | 
| Module tested with 1 and 2 rows bonded to the sensor, respectively. 
HV = 100 V
Ibias (100 V) = 27.8 nA
Ibias (200 V) = 32.7 nA | 
| Attachment 1: modul0404_1row_cal_apv0.png | 
|  | 
| Attachment 2: modul0404_1row_cal_apv1.png | 
|  | 
| Attachment 3: modul0404_1row_cmnoise_apv0.png | 
|  | 
| Attachment 4: modul0404_1row_cmnoise_apv1.png | 
|  | 
| Attachment 5: modul0404_1row_pednoise_apv0.png | 
|  | 
| Attachment 6: modul0404_1row_pednoise_apv1.png | 
|  | 
| Attachment 7: modul0404_final_cal_apv0.png | 
|  | 
| Attachment 8: modul0404_final_cal_apv1.png | 
|  | 
| Attachment 9: modul0404_final_cmnoise_apv0.png | 
|  | 
| Attachment 10: modul0404_final_cmnoise_apv1.png | 
|  | 
| Attachment 11: modul0404_final_pednoise_apv0.png | 
|  | 
| Attachment 12: modul0404_final_pednoise_apv1.png | 
|  | 
| 9 | Wed May  7 15:26:24 2008 | Christian Irmler | SPS Testbeam June08 | module | module 20/09 | properties (noise, intcal), APVs bonded to the sensor | 
| Module tested with 1 and 2 rows bonded to the sensor, respectively. 
HV = 100 V
Ibias (100 V) = 25.1 nA
Ibias (200 V) = 31.4 nA | 
| Attachment 1: modul2009_1row_cal_apv0.png | 
|  | 
| Attachment 2: modul2009_1row_cal_apv1.png | 
|  | 
| Attachment 3: modul2009_1row_cmnoise_apv0.png | 
|  | 
| Attachment 4: modul2009_1row_cmnoise_apv1.png | 
|  | 
| Attachment 5: modul2009_1row_pednoise_apv0.png | 
|  | 
| Attachment 6: modul2009_1row_pednoise_apv1.png | 
|  | 
| Attachment 7: modul2009_final_cal_apv0.png | 
|  | 
| Attachment 8: modul2009_final_cal_apv1.png | 
|  | 
| Attachment 9: modul2009_final_cmnoise_apv0.png | 
|  | 
| Attachment 10: modul2009_final_cmnoise_apv1.png | 
|  | 
| Attachment 11: modul2009_final_pednoise_apv0.png | 
|  | 
| Attachment 12: modul2009_final_pednoise_apv1.png | 
|  | 
| 8 | Wed May  7 15:40:07 2008 | Christian Irmler | SPS Testbeam June08 | module | module 07/07 | properties (noise, intcal), APVs bonded to the sensor | 
| Module tested with 1 and 2 rows bonded to the sensor, respectively. 
HV = 100 V
Ibias (100 V) = 20.2 nA
Ibias (200 V) = 21.9 nA | 
| Attachment 1: modul0707_1row_cal_apv0.png | 
|  | 
| Attachment 2: modul0707_1row_cal_apv1.png | 
|  | 
| Attachment 3: modul0707_1row_cmnoise_apv0.png | 
|  | 
| Attachment 4: modul0707_1row_cmnoise_apv1.png | 
|  | 
| Attachment 5: modul0707_1row_pednoise_apv0.png | 
|  | 
| Attachment 6: modul0707_1row_pednoise_apv1.png | 
|  | 
| Attachment 7: modul0707_final_cal_apv0.png | 
|  | 
| Attachment 8: modul0707_final_cal_apv1.png | 
|  | 
| Attachment 9: modul0707_final_cmnoise_apv0.png | 
|  | 
| Attachment 10: modul0707_final_cmnoise_apv1.png | 
|  | 
| Attachment 11: modul0707_final_pednoise_apv0.png | 
|  | 
| Attachment 12: modul0707_final_pednoise_apv1.png | 
|  | 
| 7 | Wed May  7 16:12:58 2008 | Christian Irmler | SPS Testbeam June08 | module | module 12/08 | properties (noise, intcal), APVs bonded to the sensor | 
| Module tested with 1 and 2 rows bonded to the sensor, respectively. 
HV = 100 V
Ibias (100 V) = 22.2 nA
Ibias (200 V) = 26.5 nA | 
| Attachment 1: modul1208_1row_cal_apv0.png | 
|  | 
| Attachment 2: modul0707_1row_cal_apv1.png | 
|  | 
| Attachment 3: modul0707_1row_cmnoise_apv0.png | 
|  | 
| Attachment 4: modul0707_1row_cmnoise_apv1.png | 
|  | 
| Attachment 5: modul0707_1row_pednoise_apv0.png | 
|  | 
| Attachment 6: modul0707_1row_pednoise_apv1.png | 
|  | 
| Attachment 7: modul0707_final_cal_apv0.png | 
|  | 
| Attachment 8: modul0707_final_cal_apv1.png | 
|  | 
| Attachment 9: modul0707_final_cmnoise_apv0.png | 
|  | 
| Attachment 10: modul0707_final_cmnoise_apv1.png | 
|  | 
| Attachment 11: modul0707_final_pednoise_apv0.png | 
|  | 
| Attachment 12: modul0707_final_pednoise_apv1.png | 
|  | 
| 6 | Wed May  7 15:24:49 2008 | Christian Irmler | SPS Testbeam June08 | module | module 10/02 | properties (noise, intcal), APVs bonded to the sensor | 
| Module tested with 1 and 2 rows bonded to the sensor, respectively.
HV = 100 V
Ibias (100V) = 19.1 nA
Ibias (200V) = 23.7 nA | 
| Attachment 1: modul1002_1row_cal_apv0.png | 
|  | 
| Attachment 2: modul1002_1row_cal_apv1.png | 
|  | 
| Attachment 3: modul1002_1row_cmnoise_apv0.png | 
|  | 
| Attachment 4: modul1002_1row_cmnoise_apv1.png | 
|  | 
| Attachment 5: modul1002_1row_pednoise_apv0.png | 
|  | 
| Attachment 6: modul1002_1row_pednoise_apv1.png | 
|  | 
| Attachment 7: modul1002_final_cal_apv0.png | 
|  | 
| Attachment 8: modul1002_final_cal_apv1.png | 
|  | 
| Attachment 9: modul1002_final_cmnoise_apv0.png | 
|  | 
| Attachment 10: modul1002_final_cmnoise_apv1.png | 
|  | 
| Attachment 11: modul1002_final_pednoise_apv0.png | 
|  | 
| Attachment 12: modul1002_final_pednoise_apv1.png | 
|  | 
| 5 | Wed Apr 30 16:52:17 2008 | Markus Friedl | BELLE Upgrade | module | micron | micron sensor glued to frame | 
| soeben haben wir den micron-DSSD (double metal layer) in den 2-teiligen rahmen geklebt und auf beiden seiten
temporäre kapton-stückerln aufgeklebt, über die bias appliziert werden kann. nach trocknung und bonden der