Wed Apr 23 13:05:05 2008, Christian Irmler, SPS Testbeam June08, source, hybrid 01, time correlation between TDC and sensor measurement -> 3.1 ns RMS  
 |  
|   |  
   Sun Jul  4 05:48:36 2010, Christian Irmler, BELLE Upgrade, source, Origami 6 - module 1, run002: first analysis results 7x 
 |  
Run name: run002
 
 
Run type: 0 (Hardware (Normal Run)) |  
   Wed May  7 15:24:49 2008, Christian Irmler, SPS Testbeam June08, module, module 10/02, properties (noise, intcal), APVs bonded to the sensor 12x 
 |  
Module tested with 1 and 2 rows bonded to the sensor, respectively.
 
HV = 100 V
 
Ibias (100V) = 19.1 nA
 
Ibias (200V) = 23.7 nA |  
   Wed May  7 15:26:24 2008, Christian Irmler, SPS Testbeam June08, module, module 20/09, properties (noise, intcal), APVs bonded to the sensor 12x 
 |  
Module tested with 1 and 2 rows bonded to the sensor, respectively. 
 
HV = 100 V
 
Ibias (100 V) = 25.1 nA
 
Ibias (200 V) = 31.4 nA |  
   Wed May  7 15:40:07 2008, Christian Irmler, SPS Testbeam June08, module, module 07/07, properties (noise, intcal), APVs bonded to the sensor 12x 
 |  
Module tested with 1 and 2 rows bonded to the sensor, respectively. 
 
HV = 100 V
 
Ibias (100 V) = 20.2 nA
 
Ibias (200 V) = 21.9 nA |  
   Wed May  7 16:12:58 2008, Christian Irmler, SPS Testbeam June08, module, module 12/08, properties (noise, intcal), APVs bonded to the sensor 12x 
 |  
Module tested with 1 and 2 rows bonded to the sensor, respectively. 
 
HV = 100 V
 
Ibias (100 V) = 22.2 nA
 
Ibias (200 V) = 26.5 nA |  
   Wed May  7 19:05:08 2008, Christian Irmler, SPS Testbeam June08, module, module 04/04, properties (noise, intcal), APVs bonded to the sensor 12x 
 |  
Module tested with 1 and 2 rows bonded to the sensor, respectively. 
 
HV = 100 V
 
Ibias (100 V) = 27.8 nA
 
Ibias (200 V) = 32.7 nA |  
   Fri May  9 09:56:15 2008, Christian Irmler, SPS Testbeam June08, module, module 06/03, properties (noise, intcal), APVs bonded to the sensor 12x 
 |  
Module tested with 1 and 2 rows bonded to the sensor, respectively. 
 
HV = 100 V
 
Ibias (100 V) = 26.5 nA
 
Ibias (200 V) = 37.8 nA |  
   Fri May  9 10:00:34 2008, Christian Irmler, SPS Testbeam June08, module, module 03/10, properties (noise, intcal), APVs bonded to the sensor 12x 
 |  
Module tested with 1 and 2 rows bonded to the sensor, respectively. 
 
HV = 100 V
 
Ibias (100 V) = 18.9 nA
 
Ibias (200 V) = 25.5 nA |  
   Fri May  9 10:04:26 2008, Christian Irmler, SPS Testbeam June08, module, module 05/05, properties (noise, intcal), APVs bonded to the sensor 12x 
 |  
Module tested with 1 and 2 rows bonded to the sensor, respectively. 
 
HV = 100 V
 
Ibias (100 V) = 18.0 nA
 
Ibias (200 V) = 23.6 nA |  
   Wed Apr 30 16:52:17 2008, Markus Friedl, BELLE Upgrade, module, micron, micron sensor glued to frame 
 |  
soeben haben wir den micron-DSSD (double metal layer) in den 2-teiligen rahmen geklebt und auf beiden seiten
 
temporäre kapton-stückerln aufgeklebt, über die bias appliziert werden kann. nach trocknung und bonden der
 
bias-verbindungen (montag, 5.5.2008) wird dieser für sensor-tests zur verfügung stehen. |  
   Wed Oct  7 14:23:35 2009, Dieter Uhl, BELLE Upgrade, hybrid, #4, hybrid-pitchadapter     
 |  
opens at upper coat
 
 |  
   Wed Oct  7 14:24:06 2009, Dieter Uhl, BELLE Upgrade, hybrid, #5, hybrid-pitchadapter     
 |  
shorts at upper coat
 
 |  
   Wed Apr 23 13:37:18 2008, Markus Friedl, SPS Testbeam June08, source, hybrid 01, analysis results of source test     
 |  
Ignore the "KEK November 2007" title - that's a legacy and is already changed :-)
 
 
As of now, there is no distinction in 16 separate zones. However, the gaps between the the zones are clearly visible in the Hit Profile, as the edge strips |  
   Tue May 20 14:27:50 2008, Markus Friedl, BELLE Upgrade, source, micron, analysis results of source test 9x 
 |  
 
*** NOTE: AFTER THIS MEASUREMENT WE REALIZED THAT BIASING WAS NOT DONE PROPERLY
 
          HENCE THE RESULTS BELOW ARE NOT RELIABLE 
 |  
  
   Fri May 29 11:47:56 2015, Hao Yin, Belle II, system, PS Filter, Testing PS LV filter and quantifying the required min noise lvl 
 |  
Data of this entry is recorded in the folder: LV315kHz_Injections
 
Injecting noise to LV with a freq. of 314 kHz to emulate Caen PS with KenWood PS.
 
 |  
   Thu Jun  5 10:34:29 2014, Benedikt Würkner, Belle II, source, Silc Module, Silc Angle Measurement 7° 
 |  
Measured the Silc 03/10 Module using the Sr90 Source to have a comparison for the Eta-Distribution at different angles. 
 
Data can be found on heros in: /home/medialib/LAB_Silc_Angle. 
 
Plots made with TuxOA for all different regions can be found in /home/users/bwuerkner/plots/.  |  
   Thu Jun  5 10:34:06 2014, Benedikt Würkner, Belle II, source, Silc Module, Silc Angle Measurement 4° 
 |  
Measured the Silc 03/10 Module using the Sr90 Source to have a comparison for the Eta-Distribution at different angles. 
 
Data can be found on heros in: /home/medialib/LAB_Silc_Angle. 
 
Plots made with TuxOA for all different regions can be found in /home/users/bwuerkner/plots/.  |  
   Thu Jun  5 10:33:46 2014, Benedikt Würkner, Belle II, source, Silc Module, Silc Angle Measurement 1° 
 |  
Measured the Silc 03/10 Module using the Sr90 Source to have a comparison for the Eta-Distribution at different angles. 
 
Data can be found on heros in: /home/medialib/LAB_Silc_Angle. 
 
Plots made with TuxOA for all different regions can be found in /home/users/bwuerkner/plots/.  |  
   Thu Jun  5 10:34:45 2014, Benedikt Würkner, Belle II, source, Silc Module, Silc Angle Measurement 10° 
 |  
Measured the Silc 03/10 Module using the Sr90 Source to have a comparison for the Eta-Distribution at different angles. 
 
Data can be found on heros in: /home/medialib/LAB_Silc_Angle. 
 
Plots made with TuxOA for all different regions can be found in /home/users/bwuerkner/plots/.  |  
 
 |